PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR ARGENTINA

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Argentina    
02 Population (Million) 43417 2015 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 1.215 2014 FAO
03.1 Corrugated/Packaging 0.512
03.2 Newsprint 0.115
03.3 Writing & printing 0.326
03.4 Others 0.253
04 Import 0.686
05 Export 0.080
06 Net Consumption 1.822
07 Per Capita Consumption (Kg./year/person) 42.0
08.0 Recovered Paper: Collection 0.555
08.1                              Import 0.041
08.2                              Export 0.0
08.4                              Consumption/Usage 0.596
09.0 Wood Pulp:           Production 0.749
09.1                              Import 0.151
09.2                              Export 0.185
09.4                              Consumption/Usage 0.715
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog please send me at harigoyal@yahoo.com and I will review it and publish