PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR ESTONIA

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Estonia    
02 Population (Million) 1.315 2014 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 0.076 2014 FAO

 

03.1 Corrugated/Packaging 0.071
03.2 Newsprint 0.0
03.3 Writing & printing 0.0
03.4 Others 0.005
04 Import 0.154
05 Export 0.091
06 Net Consumption 0.133
07 Per Capita Consumption (Kg./year/person) 101
08.0 Recovered Paper: Collection 0.090
08.1                              Import 0.001
08.2                              Export 0.061
08.4                              Consumption/Usage 0.030
09.0 Wood Pulp:           Production 0.240
09.1                              Import 0.028
09.2                              Export 0.174
09.4                              Consumption/Usage 0.094
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog please send me at harigoyal@yahoo.com and I will review it and publish