PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR SOUTH KOREA

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Korea (South)    
02 Population (Million) 50.61 2014 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 11.653 2014 FAO
03.1 Corrugated/Packaging 6.194
03.2 Newsprint 1.423
03.3 Writing & printing 2.557
03.4 Others 1.4
04 Import 1.004
05 Export 3.345
06 Net Consumption 9.312
07 Per Capita Consumption (Kg./year/person) 186.0
08.0 Recovered Paper: Collection 8.646
08.1                              Import 1.548
08.2                              Export 0.482
08.4                              Consumption/Usage 9.712
09.0 Wood Pulp:           Production 0.553
09.1                              Import 2.273
09.2                              Export 0.005
09.4                              Consumption/Usage 2.812
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog please send me at harigoyal@yahoo.com and I will review it and publish

Top 5 Paper & Paperboard Producing Countries  (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 400.2 110.0 111.8 398.5
China 108.8 4.6 7.3 106.0
USA 73.1 10.0 12.1 71.1
Japan 26.5 2.0 1.4 27.1
Germany 22.6 11.4 13.7 20.2
Korea Republic (South) 11.7 1.0 3.3 9.3

Top 5 Recovered Paper Producing/Collection Countries  (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 221.1 55.9 55.4 221.6
China 53.7 28.3 1.1 81.0
USA 46.4 0.78 19.1 28.1
Japan 21.8 0.0 4.6 17.2
Germany 15.1 3.96 2.4 16.7
Korea Republic (South) 8.6 1.54 0.48 9.7

Top 5 Wood Pulp Importing Countries  (Million Metric Ton in 2013)

Countries Million MT
  Production Imports Exports Net Consumption
World 397.6 107.1 109.4 395.2
China 105.1 4.8 6.8 103.1
USA 74.3 9.7 12.1 71.9
Japan 26.1 2.1 1.1 27.1
Germany 22.4 10.6 13.1 19.9
Korea Republic (South) 11.8 0.86 3.22 9.4

Top 5 Non-Wood Pulp Importing Countries (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 13.2 0.409 0.424 13.2
China 7.6 0.064 0.093 7.520
Saudi Arabia 0 0.031 0.0 0.031
Japan 0 0.028 0.0 0.033
Korea Republic (South) 0 0.025 0.0 0.025
India 2.0 0.021 0.0 2.016