PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR LITHUANIA

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Lithuania    
02 Population (Million) 2.893 2015 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 0.140 2014 FAO
03.1 Corrugated/Packaging 0.116
03.2 Newsprint  
03.3 Writing & printing  
03.4 Others 0.024
04 Import 0.292
05 Export 0.122
06 Net Consumption 0.310
07 Per Capita Consumption (Kg./year/person) 106.0
08.0 Recovered Paper: Collection 0.169
08.1                              Import 0.087
08.2                              Export 0.090
08.4                              Consumption/Usage 0.166
09.0 Wood Pulp:           Production 0.0
09.1                              Import 0.027
09.2                              Export 0.024
09.4                              Consumption/Usage 0.003
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)