PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR NETHERLANDS

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Netherlands    
02 Population (Million) 16.929 2015 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 2.767 2014 FAO
03.1 Corrugated/Packaging 1.760
03.2 Newsprint 0.253
03.3 Writing & printing 0.638
03.4 Others 0.11
04 Import 2.570
05 Export 2.246
06 Net Consumption 3.091
07 Per Capita Consumption (Kg./year/person) 183.0
08.0 Recovered Paper: Collection 2.209
08.1                              Import 2.11
08.2                              Export 2.466
08.4                              Consumption/Usage 1.852
09.0 Wood Pulp:           Production 0.044
09.1                              Import 2.395
09.2                              Export 1.679
09.4                              Consumption/Usage 0.760
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog please send me at harigoyal@yahoo.com and I will review it and publish

Top 5 Wood Pulp Importing Countries  (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 172.9 57.8 58.5 172.1
China 10.4 18.7 0.0 29.0
USA 47.8 5.8 7.9 45.7
Germany 2.6 4.7 1.3 6.0
Italy 0.41 3.4 0.0 3.8
The Netherland 0.04 2.4 1.7 0.8

Top 5 Paper & Paperboard Importing Countries  (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 400.2 110.0 111.8 398.5
Germany 22.5 11.4 13.7 20.2
USA 73.1 10.0 12.1 71.0
UK 4.4 5.5 1.1 9.3
Italy 8.6 4.9 3.3 10.1
France 8.2 4.8 4.2 8.8

Top 5 Recovered Paper  Importing Countries  (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 221.1 55.91 55.4 221.6
China 53.7 28.32 1.1 80.9
Germany 15.1 3.96 2.4 16.7
India 2.64 3.07 0 5.71
Indonesia 3.93 2.28 0.018 6.2
Netherland 2.20 2.11 2.47 1.9

Top 5 Recovered Paper Exporting Countries  (Million Metric Ton in 2014)

Countries Million MT
  Production Imports Exports Net Consumption
World 221.1 55.9 55.4 221.6
USA 46.4 0.78 19.1 28.1
Japan 21.8 0.03 4.6 17.2
UK 8.0 0.14 4.4 3.7
France 7.3 0.84 2.9 5.4
Netherland 2.2 2.11 2.5 1.9