PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR PARAGUAY

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Paraguay    
02 Population (Million) 6.80 2013 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 0.013 2014 FAO
03.1 Corrugated/Packaging 0.011
03.2 Newsprint  
03.3 Writing & printing  
03.4 Others 0.002
04 Import 0.117
05 Export 0.023
06 Net Consumption 0.106
07 Per Capita Consumption (Kg./year/person) 16.0
08.0 Recovered Paper: Collection 0.022
08.1                              Import 0.008
08.2                              Export 0.000
08.4                              Consumption/Usage 0.030
09.0 Wood Pulp:           Production  
09.1                              Import  
09.2                              Export  
09.4                              Consumption/Usage  
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)