PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR PORTUGAL

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Portugal    
02 Population (Million) 10.427 2014 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 2.177 2014 FAO
03.1 Corrugated/Packaging 0.474
03.2 Newsprint  
03.3 Writing & printing 1.560
03.4 Others 0.143
04 Import 0.820
05 Export 1.879
06 Net Consumption 1.117
07 Per Capita Consumption (Kg./year/person) 107.0
08.0 Recovered Paper: Collection 0.749
08.1                              Import 0.033
08.2                              Export 0.379
08.4                              Consumption/Usage 0.402
09.0 Wood Pulp:           Production 2.620
09.1                              Import 0.129
09.2                              Export 1.109
09.4                              Consumption/Usage 1.640
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)