PAPER & PAPERBOARD PRODUCTION & CONSUMPTION FOR VENEZUELA

HOME COUNTRY WISE STATISTICS
S.N. Particular   Time of Information Source
01 Country Venezuela    
02 Population (Million) 33.21 2014 http://en.wikipedia.org
03 Total Pulp/Paper/Paperboard Production 0.336 2014 FAO
03.1 Corrugated/Packaging 0.163
03.2 Newsprint 0.0
03.3 Writing & printing 0.039
03.4 Others 0.134
04 Import 0.247
05 Export 0.0
06 Net Consumption 0.582
07 Per Capita Consumption (Kg./year/person) 19.0
08.0 Recovered Paper: Collection 0.201
08.1                              Import 0.067
08.2                              Export 0.0
08.4                              Consumption/Usage 0.268
09.0 Wood Pulp:           Production 0.039
09.1                              Import 0.111
09.2                              Export 0.0
09.4                              Consumption/Usage 0.151
10 No. of Pulp/Paper Mills      
11 Main Raw Materials      
12 Major Companies      

All Production, Import, Export and Net Consumption numbers are in Million Metric Tons (1,000,000,000 Kg.)
Please provide if you have the latest info. If you want to write a Blog please send me at harigoyal@yahoo.com and I will review it and publish